Chemical Analysis
AISI: 303Kx +
EN: 1,4570
C max: 0,08
Mn max: 2
P max: 0,045
S max: 0,15÷0,35
Si max: 1
Cr: 17÷19
Ni: 8÷10
Mo: –
Altri: Cu = 1,4÷1,8 – N ≤ 0,11

Chemical Analysis
Characteristics
Cr-Ni austenitic steel non-hardenable, particularly suitable for welded constructions. Presents excellent intercrystalline corrosion resistance and may be used normally at temperatures of up to 425°C.
Example Of Use
The same as 304 for welded constructions and where intercrystalline corrosion resistance is required.
Quality
The quality of EUREINOX products is closely linked to the quality of raw materials used. To this end, we have been able to establish valuable relationships with the best European steel mills over the years, thereby allowing us to utilize the highest quality materials available on the market in our production lines and optimize on our experience in casting.
The complete list of products is also in Eure Inox catalogue.
EURE+ Materials