Chemical Analysis


AISI: 304Cu
EN: 1,4567
C max: 0,04
Mn max: 2
P max: 0,045
S max: 0,03
Si max: 1
Cr: 17÷19
Ni: 8,5÷10,5
Mo:
Altri: N ≤ 0,11 – Cu= 3÷4

Characteristics

Austenitic steel nonmagnetic under all conditions, the presence of Cu and Ni ensures excellent plasticity and flow, and good resistance even in sea water.

Example Of Use

Moulding of microscrews, hexagonal socket head bolts, cross-head screws.

Quality

The quality of EUREINOX products is closely linked to the quality of raw materials used. To this end, we have been able to establish valuable relationships with the best European steel mills over the years, thereby allowing us to utilize the highest quality materials available on the market in our production lines and optimize on our experience in casting.
The complete list of products is also in Eure Inox catalogue.

EURE+ Materials